您的位置: QC Procedure

QC Procedure

QC Procedure

We have several ways to QC ecah type of parts.

1.Packaging check 

whether the packaging is intact, whether the packaging meets the requirements of the order, pay attention to whether the order requires the original packaging vacuum packaging is good. MSL2-5 must MLS1&6 at will, whether the material number and quantity is correct, whether the side band is neat and firm, whether the positioning hole in the braided tape punched side, whether the component shape color is consistent, (non-polar components may not be aligned in the same direction) Whether the appearance of the label is good and the production date is reasonable Visual inspection / magnifying glass / microscope / cotton swab / acetone / scraper / vernier caliper / solderability tester / professional instruments / testing machine / oscilloscope, etc.

2.Label check 

whether the bar code is clear and scannable, whether the LOGO is correct, whether the production date meets the order requirements, whether the green environment is in line with the order requirements, whether the factory quality inspection and packaging time is correct and reasonable

3.Pin and package check. 

Check whether the color and shape of the pin solder ball is normal, (no oxidation, deformation, burr, damage, pollution, etc.) whether the package form is correct, whether the number of tube corners is correct, whether the tube corners are coplanar, whether there are scratches or pinholes on the surface, whether the resin is damaged, whether the package edge is rounded, whether there are chamfers

Screen printing check. Check whether the screen printing is correct, pay attention to the direction of screen printing specified in the product specification. The dimple and convex marks on the silkscreen, whether the positioning holes are correct and clear.

4.Surface test.

Wipe with acetone, observe whether the surface of the product and the silkscreen is faded and whether the swab becomes black

5.Scratch test. 

Whether the material scraped out with a scraper is in the form of powder

6.Product consistency.

Product consistency measurement parameter value only for capacitance resistance, inductance, etc.

7.dimension check.

Check whether the overall dimension, corner position, pin spacing and pin length are consistent with the package outline mark.

8.solderability test

Whether the solderability test pin and solder ball can be soldered normally.

9.D-CAP

Internal inspection and opening test (D-CAP). Is the internal matrix structure correct.

10.Fuction test.

whether the function and performance test function and performance test function and performance meet the specifications. Test machine, oscilloscope is equal to seven



For RMA issue.

Our offer supports as blow.

1.Customer issues RMA request

In case of material quality problems, the customer will give evidence and notify relevant sales to ask for a reply.

2.Quick response

After receiving customer information, the company set up RMA team, and contacted the corresponding suppliers and engineers within 24 hours to give solutions.

3.Recheck

After the engineers communicate with each other, the samples that need re-inspection will be sent back to our company to arrange the original factory or professional organization for testing.

4.result

According to the test results, issue relevant reports, decide whether to return or not, and if so, quickly arrange relevant procedures and inform customers.


We gurantee that:

All materials are guaranteed for one year from the date of shipment

All material photos and documents are archived for two years to ensure the traceability of materials

Provide 7*24 hours after-sales support service